Stress Corrosion Cracking of Pipelines

Download Stress Corrosion Cracking of Pipelines PDF Online Free

Author :
Publisher : John Wiley & Sons
ISBN 13 : 1118537084
Total Pages : 292 pages
Book Rating : 4.1/5 (185 download)

DOWNLOAD NOW!


Book Synopsis Stress Corrosion Cracking of Pipelines by : Y. Frank Cheng

Download or read book Stress Corrosion Cracking of Pipelines written by Y. Frank Cheng and published by John Wiley & Sons. This book was released on 2013-02-13 with total page 292 pages. Available in PDF, EPUB and Kindle. Book excerpt: Explains why pipeline stress corrosion cracking happens and how it can be prevented Pipelines sit at the heart of the global economy. When they are in good working order, they deliver fuel to meet the ever-growing demand for energy around the world. When they fail due to stress corrosion cracking, they can wreak environmental havoc. This book skillfully explains the fundamental science and engineering of pipeline stress corrosion cracking based on the latest research findings and actual case histories. The author explains how and why pipelines fall prey to stress corrosion cracking and then offers tested and proven strategies for preventing, detecting, and monitoring it in order to prevent pipeline failure. Stress Corrosion Cracking of Pipelines begins with a brief introduction and then explores general principals of stress corrosion cracking, including two detailed case studies of pipeline failure. Next, the author covers: Near-neutral pH stress corrosion cracking of pipelines High pH stress corrosion cracking of pipelines Stress corrosion cracking of pipelines in acidic soil environments Stress corrosion cracking at pipeline welds Stress corrosion cracking of high-strength pipeline steels The final chapter is dedicated to effective management and mitigation of pipeline stress corrosion cracking. Throughout the book, the author develops a number of theoretical models and concepts based on advanced microscopic electrochemical measurements to help readers better understand the occurrence of stress corrosion cracking. By examining all aspects of pipeline stress corrosion cracking—the causes, mechanisms, and management strategies—this book enables engineers to construct better pipelines and then maintain and monitor them to ensure safe, reliable energy supplies for the world.

Materials Science Research Trends

Download Materials Science Research Trends PDF Online Free

Author :
Publisher : Nova Publishers
ISBN 13 : 9781600216541
Total Pages : 370 pages
Book Rating : 4.2/5 (165 download)

DOWNLOAD NOW!


Book Synopsis Materials Science Research Trends by : Lawrence V. Olivante

Download or read book Materials Science Research Trends written by Lawrence V. Olivante and published by Nova Publishers. This book was released on 2008 with total page 370 pages. Available in PDF, EPUB and Kindle. Book excerpt: Materials science includes those parts of chemistry and physics that deal with the properties of materials. It encompasses four classes of materials, the study of each of which may be considered a separate field: metals; ceramics; polymers and composites. Materials science is often referred to as materials science and engineering because it has many applications. Industrial applications of materials science include processing techniques (casting, rolling, welding, ion implantation, crystal growth, thin-film deposition, sintering, glassblowing, etc), analytical techniques (electron microscopy, x-ray diffraction, calorimetry, nuclear microscopy (HEFIB) etc.), materials design, and cost/benefit tradeoffs in industrial production of materials. This new book presents new leading-edge research in the field.

Petroleum Abstracts

Download Petroleum Abstracts PDF Online Free

Author :
Publisher :
ISBN 13 :
Total Pages : 404 pages
Book Rating : 4.F/5 ( download)

DOWNLOAD NOW!


Book Synopsis Petroleum Abstracts by :

Download or read book Petroleum Abstracts written by and published by . This book was released on 1997 with total page 404 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Chemical Abstracts

Download Chemical Abstracts PDF Online Free

Author :
Publisher :
ISBN 13 :
Total Pages : 2566 pages
Book Rating : 4.3/5 (91 download)

DOWNLOAD NOW!


Book Synopsis Chemical Abstracts by :

Download or read book Chemical Abstracts written by and published by . This book was released on 2002 with total page 2566 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Progresses in Fracture and Strength of Materials and Structures

Download Progresses in Fracture and Strength of Materials and Structures PDF Online Free

Author :
Publisher : Trans Tech Publications Ltd
ISBN 13 : 3038131350
Total Pages : 3204 pages
Book Rating : 4.0/5 (381 download)

DOWNLOAD NOW!


Book Synopsis Progresses in Fracture and Strength of Materials and Structures by : Yu Zhou

Download or read book Progresses in Fracture and Strength of Materials and Structures written by Yu Zhou and published by Trans Tech Publications Ltd. This book was released on 2007-09-10 with total page 3204 pages. Available in PDF, EPUB and Kindle. Book excerpt: APCFS 2006 Selected, peer reviewed papers from the Asian Pacific Conference Fracture and Strength 2006 (APCFS 06), held at Sanya, Hainan Island, China during November 22~25, 2006

Corrosion-deformation Interactions CDI '96

Download Corrosion-deformation Interactions CDI '96 PDF Online Free

Author :
Publisher : Woodhead Publishing Limited
ISBN 13 :
Total Pages : 568 pages
Book Rating : 4.3/5 (91 download)

DOWNLOAD NOW!


Book Synopsis Corrosion-deformation Interactions CDI '96 by : Thierry Magnin

Download or read book Corrosion-deformation Interactions CDI '96 written by Thierry Magnin and published by Woodhead Publishing Limited. This book was released on 1997 with total page 568 pages. Available in PDF, EPUB and Kindle. Book excerpt: Published for: the European Federation of Corrosion.

Corrosion Control for Offshore Structures

Download Corrosion Control for Offshore Structures PDF Online Free

Author :
Publisher : Gulf Professional Publishing
ISBN 13 : 0124046908
Total Pages : 254 pages
Book Rating : 4.1/5 (24 download)

DOWNLOAD NOW!


Book Synopsis Corrosion Control for Offshore Structures by : Ramesh Singh

Download or read book Corrosion Control for Offshore Structures written by Ramesh Singh and published by Gulf Professional Publishing. This book was released on 2014-08-12 with total page 254 pages. Available in PDF, EPUB and Kindle. Book excerpt: A variable game changer for those companies operating in hostile, corrosive marine environments, Corrosion Control for Offshore Structures provides critical corrosion control tips and techniques that will prolong structural life while saving millions in cost. In this book, Ramesh Singh explains the ABCs of prolonging structural life of platforms and pipelines while reducing cost and decreasing the risk of failure. Corrosion Control for Offshore Structures places major emphasis on the popular use of cathodic protection (CP) combined with high efficiency coating to prevent subsea corrosion. This reference begins with the fundamental science of corrosion and structures and then moves on to cover more advanced topics such as cathodic protection, coating as corrosion prevention using mill applied coatings, field applications, and the advantages and limitations of some common coating systems. In addition, the author provides expert insight on a number of NACE and DNV standards and recommended practices as well as ISO and Standard and Test Methods. Packed with tables, charts and case studies, Corrosion Control for Offshore Structures is a valuable guide to offshore corrosion control both in terms of its theory and application. - Prolong the structural life of your offshore platforms and pipelines - Understand critical topics such as cathodic protection and coating as corrosion prevention with mill applied coatings - Gain expert insight on a number of NACE and DNV standards and recommended practices as well as ISO and Standard Test Methods.

Corrosion

Download Corrosion PDF Online Free

Author :
Publisher :
ISBN 13 :
Total Pages : 612 pages
Book Rating : 4.X/5 (6 download)

DOWNLOAD NOW!


Book Synopsis Corrosion by :

Download or read book Corrosion written by and published by . This book was released on 1997-07 with total page 612 pages. Available in PDF, EPUB and Kindle. Book excerpt: Issues include special section called Corrosion abstracts.

Stress Corrosion Cracking

Download Stress Corrosion Cracking PDF Online Free

Author :
Publisher : Elsevier
ISBN 13 : 0857093762
Total Pages : 817 pages
Book Rating : 4.8/5 (57 download)

DOWNLOAD NOW!


Book Synopsis Stress Corrosion Cracking by : V S Raja

Download or read book Stress Corrosion Cracking written by V S Raja and published by Elsevier. This book was released on 2011-09-22 with total page 817 pages. Available in PDF, EPUB and Kindle. Book excerpt: The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace

Principles of Corrosion Engineering and Corrosion Control

Download Principles of Corrosion Engineering and Corrosion Control PDF Online Free

Author :
Publisher : Elsevier
ISBN 13 : 0080480330
Total Pages : 673 pages
Book Rating : 4.0/5 (84 download)

DOWNLOAD NOW!


Book Synopsis Principles of Corrosion Engineering and Corrosion Control by : Zaki Ahmad

Download or read book Principles of Corrosion Engineering and Corrosion Control written by Zaki Ahmad and published by Elsevier. This book was released on 2006-09-18 with total page 673 pages. Available in PDF, EPUB and Kindle. Book excerpt: Corrosion is a huge issue for materials, mechanical, civil and petrochemical engineers. With comprehensive coverage of the principles of corrosion engineering, this book is a one-stop text and reference for students and practicing corrosion engineers. Highly illustrated, with worked examples and definitions, it covers basic corrosion principles, and more advanced information for postgraduate students and professionals. Basic principles of electrochemistry and chemical thermodynamics are incorporated to make the book accessible for students and engineers who do not have prior knowledge of this area. Each form of corrosion covered in the book has a definition, description, mechanism, examples and preventative methods. Case histories of failure are cited for each form. End of chapter questions are accompanied by an online solutions manual.* Comprehensively covers the principles of corrosion engineering, methods of corrosion protection and corrosion processes and control in selected engineering environments* Structured for corrosion science and engineering classes at senior undergraduate and graduate level, and is an ideal reference that readers will want to use in their professional work* Worked examples, extensive end of chapter exercises and accompanying online solutions and written by an expert from a key pretochemical university

Underground Pipeline Corrosion

Download Underground Pipeline Corrosion PDF Online Free

Author :
Publisher : Elsevier
ISBN 13 : 0857099264
Total Pages : 343 pages
Book Rating : 4.8/5 (57 download)

DOWNLOAD NOW!


Book Synopsis Underground Pipeline Corrosion by : Mark Orazem

Download or read book Underground Pipeline Corrosion written by Mark Orazem and published by Elsevier. This book was released on 2014-02-17 with total page 343 pages. Available in PDF, EPUB and Kindle. Book excerpt: Underground pipelines transporting liquid petroleum products and natural gas are critical components of civil infrastructure, making corrosion prevention an essential part of asset-protection strategy. Underground Pipeline Corrosion provides a basic understanding of the problems associated with corrosion detection and mitigation, and of the state of the art in corrosion prevention. The topics covered in part one include: basic principles for corrosion in underground pipelines, AC-induced corrosion of underground pipelines, significance of corrosion in onshore oil and gas pipelines, numerical simulations for cathodic protection of pipelines, and use of corrosion inhibitors in managing corrosion in underground pipelines. The methods described in part two for detecting corrosion in underground pipelines include: magnetic flux leakage, close interval potential surveys (CIS/CIPS), Pearson surveys, in-line inspection, and use of both electrochemical and optical probes. While the emphasis is on pipelines transporting fossil fuels, the concepts apply as well to metallic pipes for delivery of water and other liquids. Underground Pipeline Corrosion is a comprehensive resource for corrosion, materials, chemical, petroleum, and civil engineers constructing or managing both onshore and offshore pipeline assets; professionals in steel and coating companies; and academic researchers and professors with an interest in corrosion and pipeline engineering. - Reviews the causes and considers the detection and prevention of corrosion to underground pipes - Addresses a lack of current, readily available information on the subject - Case studies demonstrate how corrosion is managed in the underground pipeline industry

Corrosion in the Petrochemical Industry

Download Corrosion in the Petrochemical Industry PDF Online Free

Author :
Publisher : ASM International
ISBN 13 : 9780871705051
Total Pages : 524 pages
Book Rating : 4.7/5 (5 download)

DOWNLOAD NOW!


Book Synopsis Corrosion in the Petrochemical Industry by : Linda Garverick

Download or read book Corrosion in the Petrochemical Industry written by Linda Garverick and published by ASM International. This book was released on 1994-01-01 with total page 524 pages. Available in PDF, EPUB and Kindle. Book excerpt: A comprehensive collection of peer-reviewed data and information on corrosion in the petroleum, petrochemical, and chemical processing industries from a number of ASM International publications. The principal sources are Corrosion, Volume 13, and Failure Analysis and Prevention, Volume 11 of ASM H

Corrosion Science and Technology

Download Corrosion Science and Technology PDF Online Free

Author :
Publisher : CRC Press
ISBN 13 : 1351259903
Total Pages : 699 pages
Book Rating : 4.3/5 (512 download)

DOWNLOAD NOW!


Book Synopsis Corrosion Science and Technology by : David E.J. Talbot

Download or read book Corrosion Science and Technology written by David E.J. Talbot and published by CRC Press. This book was released on 2018-01-29 with total page 699 pages. Available in PDF, EPUB and Kindle. Book excerpt: Twenty years after its first publication, Corrosion Science and Technology continues to be a relevant practical guide for students and professionals interested in material science. This Third Edition thoroughly covers the basic principles of corrosion science in the same reader-friendly manner that made the previous edition invaluable, and enlarges the scope of the content with expanded chapters on processes for various metals and new technologies for limiting costs and metal degradation in a variety of commercial enterprises not explored in previous editions. This book also presents expertly developed methods of corrosion testing and prediction.

Stress-corrosion Cracking

Download Stress-corrosion Cracking PDF Online Free

Author :
Publisher : ASM International(OH)
ISBN 13 :
Total Pages : 466 pages
Book Rating : 4.3/5 (91 download)

DOWNLOAD NOW!


Book Synopsis Stress-corrosion Cracking by : Russell H. Jones

Download or read book Stress-corrosion Cracking written by Russell H. Jones and published by ASM International(OH). This book was released on 1992 with total page 466 pages. Available in PDF, EPUB and Kindle. Book excerpt: Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen

Comprehensive Treatise of Electrochemistry

Download Comprehensive Treatise of Electrochemistry PDF Online Free

Author :
Publisher : Springer Science & Business Media
ISBN 13 : 1468437852
Total Pages : 632 pages
Book Rating : 4.4/5 (684 download)

DOWNLOAD NOW!


Book Synopsis Comprehensive Treatise of Electrochemistry by : John Bockris

Download or read book Comprehensive Treatise of Electrochemistry written by John Bockris and published by Springer Science & Business Media. This book was released on 2013-03-09 with total page 632 pages. Available in PDF, EPUB and Kindle. Book excerpt: It is now time for a comprehensive treatise to look at the whole field of electrochemistry. The present treatise was conceived in 1974, and the earliest invitations to authors for contributions were made in 1975. The completion of the early volumes has been delayed by various factors. There has been no attempt to make each article emphasize the most recent situation at the expense of an overall statement of the modern view. This treatise is not a collection of articles from Recent Advances in Electrochemistry or Modern Aspects of Electrochemistry. It is an attempt at making a mature statement about the present position in the vast area of what is best looked at as a new interdisciplinary field. Texas A & M University J. O'M. Bockris University of Ottawa B. E. Conway Case Western Reserve University Ernest Yeager & M University Texas A Ralph E. White Preface to Volume 2 This volume brings together some dozen processes well known to the electro chemist and treats them according to their various degrees of importance. The production of hydrogen is one of the more important processes, particularly with respect to the prospects of a hydrogen economy. No one would doubt, however, that the most commercially important electrochemical processes at the present time are the production of aluminum and of chlorine. Each of these processes has a separate chapter devoted to it.

Essentials of Coating, Painting, and Lining for the Oil, Gas and Petrochemical Industries

Download Essentials of Coating, Painting, and Lining for the Oil, Gas and Petrochemical Industries PDF Online Free

Author :
Publisher : Gulf Professional Publishing
ISBN 13 : 0128016655
Total Pages : 815 pages
Book Rating : 4.1/5 (28 download)

DOWNLOAD NOW!


Book Synopsis Essentials of Coating, Painting, and Lining for the Oil, Gas and Petrochemical Industries by : Alireza Bahadori

Download or read book Essentials of Coating, Painting, and Lining for the Oil, Gas and Petrochemical Industries written by Alireza Bahadori and published by Gulf Professional Publishing. This book was released on 2015-01-06 with total page 815 pages. Available in PDF, EPUB and Kindle. Book excerpt: With the oil and gas industry facing new challenges—deeper offshore installations, more unconventional oil and gas transporting through pipelines, and refinery equipment processing these opportunity feedstocks--new corrosion challenges are appearing, and the oil and gas industry's infrastructure is only as good as the quality of protection provided and maintained. Essentials of Coating, Painting, and Linings for the Oil, Gas, and Petrochemical Industries is the first guide of its kind to directly deliver the necessary information to prevent and control corrosion for the components on the offshore rig, pipelines underground and petrochemical equipment. Written as a companion to Cathodic Corrosion Protection Systems, this must-have training tool supplies the oil and gas engineer, inspector and manager with the full picture of corrosion prevention methods specifically catered for oil and gas services. Packed with real world case studies, critical qualifications, inspection criteria, suggested procedure tests, and application methods, Essentials of Coating, Painting, and Linings for the Oil, Gas and Petrochemical Industries is a required straightforward reference for any oil and gas engineer and manager. - Understand how to select, prime and apply the right coating system for various oil and gas equipment and pipelines – both upstream and downstream - Train personnel with listed requirements, evaluation material and preparation guides, including important environmental compliance considerations - Improve the quality of your equipment, refinery and pipeline with information on repair and rejection principles

Applied Metallurgy and Corrosion Control

Download Applied Metallurgy and Corrosion Control PDF Online Free

Author :
Publisher : Springer
ISBN 13 : 9811046840
Total Pages : 558 pages
Book Rating : 4.8/5 (11 download)

DOWNLOAD NOW!


Book Synopsis Applied Metallurgy and Corrosion Control by : Amiya Kumar Lahiri

Download or read book Applied Metallurgy and Corrosion Control written by Amiya Kumar Lahiri and published by Springer. This book was released on 2017-08-23 with total page 558 pages. Available in PDF, EPUB and Kindle. Book excerpt: This book serves as a comprehensive resource on metals and materials selection for the petrochemical industrial sector. The petrochemical industry involves large scale investments, and to maintain profitability the plants are to be operated with minimum downtime and failure of equipment, which can also cause safety hazards. To achieve this objective proper selection of materials, corrosion control, and good engineering practices must be followed in both the design and the operation of plants. Engineers and professional of different disciplines involved in these activities are required to have some basic understanding of metallurgy and corrosion. This book is written with the objective of servings as a one-stop shop for these engineering professionals. The book first covers different metallic materials and their properties, metal forming processes, welding, and corrosion and corrosion control measures. This is followed by considerations in material selection and corrosion control in three major industrial sectors, oil & gas production, oil refinery, and fertilizers. The importance of pressure vessel codes as well as inspection and maintenance repair practices have also been highlighted. The book will be useful for technicians and entry level engineers in these industrial sectors. Additionally, the book may also be used as primary or secondary reading for graduate and professional coursework.